Table of Contents
Thistle Bonding Coat is an ideal base coat plaster for smooth or low suction backgrounds such as tiling, concrete, plasterboard or surfaces treated with Thistle Bond-it. The fine mix allows for improved workability, making it easier to spread, rule and Darby.
What do you use bonding plaster for?
Bonding helps plasterers achieve a smooth finish by providing a key as it simply sticks well to the surfaces it is applied to. In addition to using bonding plaster as a base coat for surfaces which will be plastered with a skim layer or polished afterwards, it can also be used on surfaces like concrete too.
How long does Thistle bonding last?
Bonding about 2-3 hours, but some do leave it to following day before skimming depends on size of area. The 3-4 days is a guide, the colour of the plaster will tell you when it’s dry enough to paint. Need to leave decent time between paint coats, for each to throughly dry before applying the next one.
How much does a bag of bonding cover?
bags the coverage is 4-6 square metres per 25kg.
Do I need bonding plaster?
5 Answers from MyBuilder Plasterers If your referring to “bonding” as in a bonding coat of plaster then your answer is no. The wall will need a coat of Pva to reduce suction from the surface in preparation for skimming.
Can I plaster without PVA?
The correct mix for pva for plastering is 1 part pva to 5 parts water, and really only used to stop the plaster drying too quickly, plastering over silk paint with or without pva can only be as adhering as the paint before, pva doesnt make the plaster stick to the behind of a painted surface!Feb 17, 2011
Why is my bonding plaster cracking?
one further thought, bonding coat will crack if you apply it too thickly as it loses a larger proportion of its volume through moisture loss. it should ideally be applied in layers no thicker than 11mm. if it requires more then build up in successive layers rather than trying to get the desired result in one hit.
What is the difference between Hardwall and bonding?
Bonding– it is a gypsum based undercoat plaster for low suction backgrounds like tiling, dense concrete blocks, engineering bricks, concrete, plasterboard surfaces. Hardwall- it is a gypsum based undercoat plaster used for more absorbent surfaces (mostly on masonry) than bonding.
Which plaster is best for walls?
Cement plaster is the best bet when it comes to plastering exterior walls because it is moisture-resistant and will protect the wall against climate changes as well as environmental pollution. Moreover the durability factor in cement plaster makes it the ideal choice for internal plastering too.
Can I use bonding plaster to fill holes?
Bonding coat can fill large holes/chunks. It’s all in the mix – your looking for a whipped cream consistency. I find it makes it very easy to apply. Slap it on and leave it rough, don’t try to finish it when it’s just been applied.
Why is lime plaster no longer commonly used?
Non-hydraulic lime plaster requires moisture to set and has to be prevented from drying for several days. The number of qualified tradesmen capable of plastering with lime is in decline due to widespread adoption of drywall and gypsum veneer plaster.
Should I PVA brickwork before bonding?
If, however, the bonding cost is pretty smooth and hasn’t got a good ‘key’ for a finishing coat to adhere to then there’s no harm in putting PVA on. You won’t need to re-moisten it before the finishing coat as long as it’s tacky, if it’s not then put another coat of 50/50 PVA/water on.
How thick can you put bonding on?
Floating coats should be applied at a thickness of 8mm, up to a total plaster thickness of 25mm, and wire scratched between each coat. The final floating coat should be ruled to an even surface and lightly scratched to form a key for Thistle finish plaster, such as Thistle MultiFinish.
Is Thistle undercoat plaster the same as bonding?
Thistle Undercoat Plaster is a gypsum undercoat plaster for use in the repair of low suction backgrounds, e.g. some brickwork, blockwork or concrete, Gyproc plasterboard, expanded metal lath, or surfaces treated with bonding agents.
Can I paint over bonding plaster?
If you have some multifinish at hand, I’d put a skim coat of that on top of the bonding first, but if you don’t then go right ahead and paint the bond coat directly. It’ll soak up your paint, so you should probably put on a couple of layers of diluted paint first mainly to seal it.
How long does it take for undercoat plaster to dry?
Fresh plaster will take 2-3 days to dry when applied to plasterboard and around 7 days to dry when applied with a backing plaster or undercoat.
Can I use bonding plaster on plasterboard?
To put it into context – standard plasterboard is the same – this will also not withstand continued dampness but is fine on a bathroom ceiling. One coat of bonding coat over your existing plasterboards (sealed with PVA if in doubt) can then be ruled flat with a straight edge.
Do you need to PVA before bonding plaster?
PVA for Bonding Adding a coat of the glue to your wall surface just before you start plastering helps to bond the plaster to the wall. The PVA literally helps to stick the plaster in place in the same way it can bond two pieces of wood together.
Can you use out of date Thistle bonding?
If it is mixed up and shaped before the final setting, then it should be fine. If it starts to go stiff whilst on the trowel, and you still spread it out, you are actually working with half-set plaster, so it’ll only ultimately fully set to half (ish) its normal strength.